Liu, Y., Bi, C., Gao, Y., Gyakari, F. N., & Zha, X. (2026). Role of Reactive Silica Addition in Enhancing Geopolymerization Efficiency and Strength Development of Calcined Granite Waste. Materials (1996-1944), 19(5), 886. https://doi.org/10.3390/ma19050886