The optimization of the strontium compounds production, using a celestine ore sample.

Saved in:
Bibliographic Details
Title: The optimization of the strontium compounds production, using a celestine ore sample.
Alternate Title: Optimizacija proizvodnje stroncijevih spojeva pomoću uzorka celestinske rude.
Authors: Alishahi, Ardalan1, Noaparast, Mohammad1 Noparast@ut.ac.ir, Ashani, Ali Rezaei1, Nasab, Marzieh Hosseini2
Source: Rudarsko-Geološko-Naftni Zbornik. 2023, Vol. 38 Issue 4, p53-62. 10p.
Subject Terms: *Strontium compounds, *Sodium carbonate, *Dimensional analysis, *Strontium, *Ores, *Strontium oxide
Abstract (English): The direct conversion of celestine (SrSO4) to strontium carbonate as well as its enrichment by hydrometallurgy were investigated. A study was also conducted to investigate whether acid concentration affected the quality of strontium sulfate in celestine concentrates. Based on the results of a laboratory assay, it was determined that 98.04% SrSO4 was leached optimally under agitation. The ground sample of celestine concentrate was then leached by agitation for three hours after the dimensional analysis had determined the appropriate grinding time. To determine the optimal approach for the agitated leaching of strontium carbonate, different approaches were tested. Various factors, including temperature, return water, solid percentage, and sodium carbonate to strontium sulfate ratio, were studied. At 90°C, celestine completely converts into strontium carbonate with a solid percentage of 20% and a sodium carbonate to strontium sulfate ratio of 4:5. As part of the investigation into the possibility of producing strontium oxide, samples of celestine concentrate and strontium carbonate produced under optimal conditions were heated at 500 and 1000°C to determine which phase would form the oxidized phase. An X-ray analysis indicates that the oxidation phase forms at a temperature of more than 750°C. [ABSTRACT FROM AUTHOR]
Abstract (Croatian): U radu se istražuje izravna pretvorba celestina (SrSO4) u stroncijev karbonat i njegovo obogaćivanje hidrometalurgijskim postupcima. Također, provedeno je istraživanje o utjecaju koncentracije kiseline na kvalitetu stroncijeva sulfata u koncentratima celestina. Na temelju rezultata laboratorijskih ispitivanja utvrđeno je da se 98,04 % SrSO4 optimalno izlužuje uz miješanje. Nakon što je dimenzijskom analizom određeno odgovarajuće vrijeme mljevenja, samljeveni uzorak koncentrata celestina izlužen je protresanjem tijekom tri sata. Testirani su različiti pristupi kako bi se odredio optimalan postupak za izluživanje uz protresanje stroncijeva karbonata. Proučavani su različiti čimbenici, uključujući temperaturu, povratnu vodu, postotak čvrste tvari i omjer natrijeva karbonata i stroncijeva sulfata. Na 90 °C celestin se potpuno pretvara u stroncijev karbonat s 20 % udjela čvrste tvari i omjerom natrijeva karbonata i stroncijeva sulfata od 4 : 5. Kako bi se utvrdilo koja će faza tvoriti oksidiranu fazu u sklopu istraživanja mogućnosti proizvodnje stroncijeva oksida, uzorci koncentrata celestina i stroncijeva karbonata načinjeni su u optimalnim uvjetima zagrijavanjem na 500 i 1000 °C. Rendgenska analiza pokazuje da se oksidacijska faza formira na temperaturi višoj od 750 °C. [ABSTRACT FROM AUTHOR]
Database: Energy & Power Source
FullText Links:
  – Type: pdflink
Text:
  Availability: 0
Header DbId: enr
DbLabel: Energy & Power Source
An: 174146879
AccessLevel: 6
PubType: Academic Journal
PubTypeId: academicJournal
PreciseRelevancyScore: 0
IllustrationInfo
Items – Name: Title
  Label: Title
  Group: Ti
  Data: The optimization of the strontium compounds production, using a celestine ore sample.
– Name: TitleAlt
  Label: Alternate Title
  Group: TiAlt
  Data: Optimizacija proizvodnje stroncijevih spojeva pomoću uzorka celestinske rude.
– Name: Author
  Label: Authors
  Group: Au
  Data: <searchLink fieldCode="AR" term="%22Alishahi%2C+Ardalan%22">Alishahi, Ardalan</searchLink><relatesTo>1</relatesTo><br /><searchLink fieldCode="AR" term="%22Noaparast%2C+Mohammad%22">Noaparast, Mohammad</searchLink><relatesTo>1</relatesTo><i> Noparast@ut.ac.ir</i><br /><searchLink fieldCode="AR" term="%22Ashani%2C+Ali+Rezaei%22">Ashani, Ali Rezaei</searchLink><relatesTo>1</relatesTo><br /><searchLink fieldCode="AR" term="%22Nasab%2C+Marzieh+Hosseini%22">Nasab, Marzieh Hosseini</searchLink><relatesTo>2</relatesTo>
– Name: TitleSource
  Label: Source
  Group: Src
  Data: <searchLink fieldCode="JN" term="%22Rudarsko-Geološko-Naftni+Zbornik%22">Rudarsko-Geološko-Naftni Zbornik</searchLink>. 2023, Vol. 38 Issue 4, p53-62. 10p.
– Name: Subject
  Label: Subject Terms
  Group: Su
  Data: *<searchLink fieldCode="DE" term="%22Strontium+compounds%22">Strontium compounds</searchLink><br />*<searchLink fieldCode="DE" term="%22Sodium+carbonate%22">Sodium carbonate</searchLink><br />*<searchLink fieldCode="DE" term="%22Dimensional+analysis%22">Dimensional analysis</searchLink><br />*<searchLink fieldCode="DE" term="%22Strontium%22">Strontium</searchLink><br />*<searchLink fieldCode="DE" term="%22Ores%22">Ores</searchLink><br />*<searchLink fieldCode="DE" term="%22Strontium+oxide%22">Strontium oxide</searchLink>
– Name: Abstract
  Label: Abstract (English)
  Group: Ab
  Data: The direct conversion of celestine (SrSO4) to strontium carbonate as well as its enrichment by hydrometallurgy were investigated. A study was also conducted to investigate whether acid concentration affected the quality of strontium sulfate in celestine concentrates. Based on the results of a laboratory assay, it was determined that 98.04% SrSO4 was leached optimally under agitation. The ground sample of celestine concentrate was then leached by agitation for three hours after the dimensional analysis had determined the appropriate grinding time. To determine the optimal approach for the agitated leaching of strontium carbonate, different approaches were tested. Various factors, including temperature, return water, solid percentage, and sodium carbonate to strontium sulfate ratio, were studied. At 90°C, celestine completely converts into strontium carbonate with a solid percentage of 20% and a sodium carbonate to strontium sulfate ratio of 4:5. As part of the investigation into the possibility of producing strontium oxide, samples of celestine concentrate and strontium carbonate produced under optimal conditions were heated at 500 and 1000°C to determine which phase would form the oxidized phase. An X-ray analysis indicates that the oxidation phase forms at a temperature of more than 750°C. [ABSTRACT FROM AUTHOR]
– Name: Abstract
  Label: Abstract (Croatian)
  Group: Ab
  Data: U radu se istražuje izravna pretvorba celestina (SrSO4) u stroncijev karbonat i njegovo obogaćivanje hidrometalurgijskim postupcima. Također, provedeno je istraživanje o utjecaju koncentracije kiseline na kvalitetu stroncijeva sulfata u koncentratima celestina. Na temelju rezultata laboratorijskih ispitivanja utvrđeno je da se 98,04 % SrSO4 optimalno izlužuje uz miješanje. Nakon što je dimenzijskom analizom određeno odgovarajuće vrijeme mljevenja, samljeveni uzorak koncentrata celestina izlužen je protresanjem tijekom tri sata. Testirani su različiti pristupi kako bi se odredio optimalan postupak za izluživanje uz protresanje stroncijeva karbonata. Proučavani su različiti čimbenici, uključujući temperaturu, povratnu vodu, postotak čvrste tvari i omjer natrijeva karbonata i stroncijeva sulfata. Na 90 °C celestin se potpuno pretvara u stroncijev karbonat s 20 % udjela čvrste tvari i omjerom natrijeva karbonata i stroncijeva sulfata od 4 : 5. Kako bi se utvrdilo koja će faza tvoriti oksidiranu fazu u sklopu istraživanja mogućnosti proizvodnje stroncijeva oksida, uzorci koncentrata celestina i stroncijeva karbonata načinjeni su u optimalnim uvjetima zagrijavanjem na 500 i 1000 °C. Rendgenska analiza pokazuje da se oksidacijska faza formira na temperaturi višoj od 750 °C. [ABSTRACT FROM AUTHOR]
PLink https://search.ebscohost.com/login.aspx?direct=true&site=eds-live&db=enr&AN=174146879
RecordInfo BibRecord:
  BibEntity:
    Identifiers:
      – Type: doi
        Value: 10.17794/rgn.2023.4.5
    Languages:
      – Code: eng
        Text: English
    PhysicalDescription:
      Pagination:
        PageCount: 10
        StartPage: 53
    Subjects:
      – SubjectFull: Strontium compounds
        Type: general
      – SubjectFull: Sodium carbonate
        Type: general
      – SubjectFull: Dimensional analysis
        Type: general
      – SubjectFull: Strontium
        Type: general
      – SubjectFull: Ores
        Type: general
      – SubjectFull: Strontium oxide
        Type: general
    Titles:
      – TitleFull: The optimization of the strontium compounds production, using a celestine ore sample.
        Type: main
  BibRelationships:
    HasContributorRelationships:
      – PersonEntity:
          Name:
            NameFull: Alishahi, Ardalan
      – PersonEntity:
          Name:
            NameFull: Noaparast, Mohammad
      – PersonEntity:
          Name:
            NameFull: Ashani, Ali Rezaei
      – PersonEntity:
          Name:
            NameFull: Nasab, Marzieh Hosseini
    IsPartOfRelationships:
      – BibEntity:
          Dates:
            – D: 01
              M: 08
              Text: 2023
              Type: published
              Y: 2023
          Identifiers:
            – Type: issn-print
              Value: 03534529
          Numbering:
            – Type: volume
              Value: 38
            – Type: issue
              Value: 4
          Titles:
            – TitleFull: Rudarsko-Geološko-Naftni Zbornik
              Type: main
ResultId 1