Iron Removal from Zinc Leaching Solution with High Sulfate Concentration via Hydrothermal Mineralization Precipitation at 150−160°C.

Saved in:
Bibliographic Details
Title: Iron Removal from Zinc Leaching Solution with High Sulfate Concentration via Hydrothermal Mineralization Precipitation at 150−160°C.
Authors: Peng, Xiaohua1,2, Yang, Bo1,2, Li, Xingbin1,2, lixingbin2018@163.com, Dai, Xingzheng1,3, Wei, Chang1,2, Lu, Zhanqing1,3, Deng, Zhigan1,2, Li, Minting1,2
Source: JOM: The Journal of The Minerals, Metals & Materials Society (TMS); Sep2025, Vol. 77 Issue 9, p6727-6743, 17p
Database: Applied Science & Technology Source
Full text is not displayed to guests.
Description
ISSN:10474838
DOI:10.1007/s11837-025-07546-1