Iron Removal from Zinc Leaching Solution with High Sulfate Concentration via Hydrothermal Mineralization Precipitation at 150−160°C.
Saved in:
| Title: | Iron Removal from Zinc Leaching Solution with High Sulfate Concentration via Hydrothermal Mineralization Precipitation at 150−160°C. |
|---|---|
| Authors: | Peng, Xiaohua1,2, Yang, Bo1,2, Li, Xingbin1,2, lixingbin2018@163.com, Dai, Xingzheng1,3, Wei, Chang1,2, Lu, Zhanqing1,3, Deng, Zhigan1,2, Li, Minting1,2 |
| Source: | JOM: The Journal of The Minerals, Metals & Materials Society (TMS); Sep2025, Vol. 77 Issue 9, p6727-6743, 17p |
| Database: | Applied Science & Technology Source |
|
Full text is not displayed to guests.
Login for full access.
|
|
| ISSN: | 10474838 |
|---|---|
| DOI: | 10.1007/s11837-025-07546-1 |