The tensile strength of 339 aluminum reinforced with Kaowool fibers: acomparison of T5 and T6 heat treatments.

Saved in:
Bibliographic Details
Title: The tensile strength of 339 aluminum reinforced with Kaowool fibers: acomparison of T5 and T6 heat treatments.
Authors: Baxter, William J., Sachdev, Anil K.
Source: Metallurgical & Materials Transactions. Part A; July 1999, Vol. 30A Issue 7, p1835-1841, 7p
Database: Applied Science & Technology Source
Description
ISSN:10735623
DOI:10.1007/s11661-999-0182-x