Scalable mesoporous silicon microparticles composed of interconnected nanoplates for superior lithium storage.

Saved in:
Bibliographic Details
Title: Scalable mesoporous silicon microparticles composed of interconnected nanoplates for superior lithium storage.
Authors: Mu, Tiansheng1 (AUTHOR), Shen, Baicheng1 (AUTHOR), Lou, Shuaifeng1 (AUTHOR), Zhang, Zhiguo1 (AUTHOR), Ren, Yang1 (AUTHOR), Zhou, Xiaoming1 (AUTHOR), Zuo, Pengjian1 (AUTHOR), Du, Chunyu1 (AUTHOR), Ma, Yulin1 (AUTHOR), Huo, Hua1 (AUTHOR), Yin, Geping1 (AUTHOR) yingeping@hit.edu.cn
Source: Chemical Engineering Journal. Nov2019, Vol. 375, pN.PAG-N.PAG. 1p.
Subjects: Nanosilicon, Glass waste, Lithium-ion batteries, Silicon, Lithium ions
Abstract: • MP-Si is obtained through magnesiothermic reduction reaction driven from waste glass. • Micron-sized MP-Si is composed of numerous interconnected 2D nanoplates. • MP-Si possesses abundant mesoporous structure. • MP-Si anode exhibits high reversible capacity and excellent rate capability. Constructing micro-nano hierarchical porous structure is an effective strategy to solve key issues arising from the large volume change of silicon-based materials during cycling. Herein, we successfully obtain the mesoporous silicon microparticles composed of nanoplates driven from waste glass by the magnesiothermic reduction reaction. The two-dimensional nanoplates and abundant mesoporous structure in the microparticles not only effectively mitigate the mechanical strains caused by volume changes but also promote lithium ion diffusion. The silicon microparticles display outstanding lithium storage performance including extremely high first Coulombic efficiency (85.1%), remarkable reversible specific and volumetric capacities (1793 mAh g−1 and 747 mAh cm−3 after 120 cycles at 200 mA g−1, 1000 mAh g−1 after 360 cycles at 500 mA g−1) and impressive rate performance (1183.7 mA h g−1 at 1 A g−1). Simultaneously, the corresponding electrode exhibits significantly less impedance build-up and smaller electrode thickness increase than that of commercial silicon nanoparticles. Furthermore, the scalable and cost-effective method makes it an attractive candidate for next generation lithium ion batteries anode materials. [ABSTRACT FROM AUTHOR]
Copyright of Chemical Engineering Journal is the property of Elsevier B.V. and its content may not be copied or emailed to multiple sites without the copyright holder's express written permission. Additionally, content may not be used with any artificial intelligence tools or machine learning technologies. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
Database: Engineering Source
Description
Abstract:• MP-Si is obtained through magnesiothermic reduction reaction driven from waste glass. • Micron-sized MP-Si is composed of numerous interconnected 2D nanoplates. • MP-Si possesses abundant mesoporous structure. • MP-Si anode exhibits high reversible capacity and excellent rate capability. Constructing micro-nano hierarchical porous structure is an effective strategy to solve key issues arising from the large volume change of silicon-based materials during cycling. Herein, we successfully obtain the mesoporous silicon microparticles composed of nanoplates driven from waste glass by the magnesiothermic reduction reaction. The two-dimensional nanoplates and abundant mesoporous structure in the microparticles not only effectively mitigate the mechanical strains caused by volume changes but also promote lithium ion diffusion. The silicon microparticles display outstanding lithium storage performance including extremely high first Coulombic efficiency (85.1%), remarkable reversible specific and volumetric capacities (1793 mAh g−1 and 747 mAh cm−3 after 120 cycles at 200 mA g−1, 1000 mAh g−1 after 360 cycles at 500 mA g−1) and impressive rate performance (1183.7 mA h g−1 at 1 A g−1). Simultaneously, the corresponding electrode exhibits significantly less impedance build-up and smaller electrode thickness increase than that of commercial silicon nanoparticles. Furthermore, the scalable and cost-effective method makes it an attractive candidate for next generation lithium ion batteries anode materials. [ABSTRACT FROM AUTHOR]
ISSN:13858947
DOI:10.1016/j.cej.2019.121923