The Effects of Soft-Segment Molecular Weight on the Structure and Properties of Poly(trimethylene terephthalate)-block-poly(tetramethylene glycol) Copolymers.

Saved in:
Bibliographic Details
Title: The Effects of Soft-Segment Molecular Weight on the Structure and Properties of Poly(trimethylene terephthalate)-block-poly(tetramethylene glycol) Copolymers.
Authors: Dong, Hailiang1,2 (AUTHOR), Tian, Yuchuang2 (AUTHOR), Li, Junyu1,2 (AUTHOR), Shi, Jiyou2 (AUTHOR), Kuang, Jun2 (AUTHOR), Zhou, Wenle2 (AUTHOR), Chen, Ye1 (AUTHOR)
Source: Polymers (20734360). Oct2025, Vol. 17 Issue 20, p2781. 15p.
Subjects: Block copolymers, Molecular weights, Biopolymers, Thermal properties, Microstructure, Biomaterials, Polyethylene terephthalate, Mechanical behavior of materials
Abstract: A series of PTT-b-PTMG copolyesters was synthesized via direct esterification followed by melt polycondensation using purified terephthalic acid (PTA), bio-based 1,3-propanediol (PDO), and poly(tetramethylene glycol) (PTMG) of varying molecular weights (650–3000 g/mol). The resulting materials were comprehensively characterized in terms of chemical structure, molecular weight, thermal behavior, phase morphology, crystalline architecture, and mechanical performance using a range of analytical techniques: Fourier-transform infrared spectroscopy (FTIR), 1H-NMR, gel permeation chromatography (GPC), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), wide-angle X-ray scattering (WAXS), small-angle X-ray scattering (SAXS), dynamic mechanical thermal analysis (DMA), tensile testing, and other standard physical methods. FTIR, 1H-NMR, and GPC data confirmed the successful incorporation of both PTT-hard and PTMG-soft segments into the copolymer backbone. As the PTMG molecular weight increased, the average sequence length of the PTT-hard segments (Ln,T) also increased, leading to higher melting (Tm) and crystallization (Tc) temperatures, albeit with a slight reduction in overall crystallinity. DMA results indicated enhanced microphase separation between hard and soft domains with increasing PTMG molecular weight. WAXS and SAXS analyses further revealed that the crystalline structure and long-range ordering were strongly dependent on the copolymer composition and block architecture. Mechanical testing showed that tensile strength at break remained relatively constant across the series, while Young's modulus increased significantly with higher PTMG molecular weight—concurrently accompanied by a decrease in elongation at break. Furthermore, the elastic deformability and recovery behavior of PTT-b-PTMG block copolymers were evaluated through cyclic tensile testing. TGA confirmed that all copolyesters exhibited excellent thermal stability. This study demonstrates that the physical and mechanical properties of bio-based PTT-b-PTMG elastomers can be effectively tailored by adjusting the molecular weight of the PTMG-soft segment, offering valuable insights for the rational design of sustainable thermoplastic elastomers with tunable performance. [ABSTRACT FROM AUTHOR]
Copyright of Polymers (20734360) is the property of MDPI and its content may not be copied or emailed to multiple sites without the copyright holder's express written permission. Additionally, content may not be used with any artificial intelligence tools or machine learning technologies. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
Database: Engineering Source
Full text is not displayed to guests.
Description
Abstract:A series of PTT-b-PTMG copolyesters was synthesized via direct esterification followed by melt polycondensation using purified terephthalic acid (PTA), bio-based 1,3-propanediol (PDO), and poly(tetramethylene glycol) (PTMG) of varying molecular weights (650–3000 g/mol). The resulting materials were comprehensively characterized in terms of chemical structure, molecular weight, thermal behavior, phase morphology, crystalline architecture, and mechanical performance using a range of analytical techniques: Fourier-transform infrared spectroscopy (FTIR), 1H-NMR, gel permeation chromatography (GPC), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), wide-angle X-ray scattering (WAXS), small-angle X-ray scattering (SAXS), dynamic mechanical thermal analysis (DMA), tensile testing, and other standard physical methods. FTIR, 1H-NMR, and GPC data confirmed the successful incorporation of both PTT-hard and PTMG-soft segments into the copolymer backbone. As the PTMG molecular weight increased, the average sequence length of the PTT-hard segments (Ln,T) also increased, leading to higher melting (Tm) and crystallization (Tc) temperatures, albeit with a slight reduction in overall crystallinity. DMA results indicated enhanced microphase separation between hard and soft domains with increasing PTMG molecular weight. WAXS and SAXS analyses further revealed that the crystalline structure and long-range ordering were strongly dependent on the copolymer composition and block architecture. Mechanical testing showed that tensile strength at break remained relatively constant across the series, while Young's modulus increased significantly with higher PTMG molecular weight—concurrently accompanied by a decrease in elongation at break. Furthermore, the elastic deformability and recovery behavior of PTT-b-PTMG block copolymers were evaluated through cyclic tensile testing. TGA confirmed that all copolyesters exhibited excellent thermal stability. This study demonstrates that the physical and mechanical properties of bio-based PTT-b-PTMG elastomers can be effectively tailored by adjusting the molecular weight of the PTMG-soft segment, offering valuable insights for the rational design of sustainable thermoplastic elastomers with tunable performance. [ABSTRACT FROM AUTHOR]